SmithBuilt Project: Sight Glass: Polishing the Countertops

Once the molds have been carefully removed, we check for voids and begin the polishing operation.

After the molds have been removed, Justin and Jerad begin the polishing process with a Diamond embedded grit pad.

Water polishing the counters- starts with a 200 grit pad and moves through the grits to finish at 800 grit before the sealing process.